Continuum damage mechanics for sintered powder metals

Sintered metals are characterized by the high porosity (⩾ 8%) and voids/micro-cracks in microns. Inelastic behavior of the materials is coupled with micro-crack propagation and coalescence of open voids. In the present work the damage evolution of the sintered iron under multi-axial monotonic loadin...