Effect of heat treatment on the properties of sintered nickel-molybdenum and nickel-chromium-molybdenum alloys

1. Tempering at 750–800°C severely embrittles the sintered Ni-30% Mo alloy and reduces its corrosion resistance. By employing the method of electrical resistivity measurement, it is possible rapidly to assess the structural state of the alloy and the extent of its losses of corrosion resistance and...

Ausführliche Beschreibung

Bibliographische Detailangaben
Veröffentlicht in:Powder metallurgy and metal ceramics, Vol. 10, No. 12 (1971), p. 974-977
1. Verfasser: Solonin, M.
Weitere beteiligte Personen: Chernyshev, I. ; Fedorchenko, M.
Format: elektronischer Aufsatz
Sprache:English
ISSN:1573-9066
Anmerkung:Translated from Poroshkovaya Metallurgiya, No. 12 (108), pp. 44–48, December, 1971.